Performance Standard |
Standard Repair |
| Cracks in stucco |
Hairline cracks if not excessively
numerous are acceptable. If crack exceeds 3/32" it
is unacceptable and should be repaired. |
Determine cause of crack and repair. |
| Stucco falling or chipping
around window and door frames and weep screed |
Some chipping of these areas is normal. |
None if within tolerance as determined
by Fieldstone. |
| Applied stucco is too thin
and wire lath is visible |
None acceptable. |
Make appropriate repairs. |
| There are voids in the stucco
at beams or columns |
None acceptable. |
Repair so that all surfaces are covered. |
| Stud locations visible on
stucco wall |
None acceptable. |
Repair by proper method. |